GENEVA, June 18 -- VITRIVAX, INC. (5435 Airport Boulevard, Suite 106Boulder, Colorado 80301) filed a patent application (PCT/US2024/058293) for "COMPOSITIONS, METHODS AND USES FOR DETERMINING ATOMIC LAYER DEPOSITION COATING QUALITY AND DISSOLUTION RATES" on Dec 03, 2024. With publication no. WO/2025/122516, the details related to the patent application was published on Jun 12, 2025.
Notably, the patent application was submitted under the International Patent Classification (IPC) system, which is managed by the World Intellectual Property Organization (WIPO).
Inventor(s): STEADMAN, Bryan L. (c/o VitriVax, Inc.5435 Airport Boulevard, Suite 106Boulder, Colorado 80301), NAPOLITANO, Lorena R.A. (c/o VitriVax, Inc.5435 Airport Boulevard, Suite ...