GENEVA, Oct. 18 -- SIEMENS ENERGY GLOBAL GMBH & CO. KG (Otto-Hahn-Ring 681739 Munchen) filed a patent application (PCT/EP2025/055221) for "A LOW DENSITY NICKEL BASE GAMMA PRIME STRENGTHENED SUPERALLOY, A COMPONENT AND METHOD" on Feb 26, 2025. With publication no. WO/2025/214648, the details related to the patent application was published on Oct 16, 2025.
Notably, the patent application was submitted under the International Patent Classification (IPC) system, which is managed by the World Intellectual Property Organization (WIPO).
Inventor(s): HASSELQVIST, Magnus (Torgvagen 1061213 Finspang)
Abstract: The invention is a Nickel base gamma prime strengthened superalloy with a composition (in wt%) comprising (in wt%) 3.0 - 13.0 Cobalt (Co), ...