GENEVA, Oct. 19 -- SAFRAN AIRCRAFT ENGINES (2 Boulevard Du General Martial Valin75015 PARIS) filed a patent application (PCT/FR2025/050189) for "METHOD FOR PRODUCING WELDING OR FACING RODS OF WHICH THE FILLER MATERIAL IS A METAL SUPERALLOY" on Mar 12, 2025. With publication no. WO/2025/215310, the details related to the patent application was published on Oct 16, 2025.
Notably, the patent application was submitted under the International Patent Classification (IPC) system, which is managed by the World Intellectual Property Organization (WIPO).
Inventor(s): PIETTE, Romaric Jean-Marie (Safranc/o Centre d'Excellence Propriete IntellectuelleRond-point Rene Ravaud, Reau77550 MOISSY-CRAMAYEL), SOULLIER, David Daniel (Safranc/o Cnetre d'Excelle...