GENEVA, Feb. 10 -- SAFRAN AIRCRAFT ENGINES (2 boulevard du General Martial Valin75015 PARIS) filed a patent application (PCT/FR2024/051037) for "METHOD FOR DETECTING FRECKLE-TYPE ANOMALIES IN A SAMPLE MADE OF A NICKEL-BASED SUPERALLOY" on Jul 26, 2024. With publication no. WO/2025/027252, the details related to the patent application was published on Feb 06, 2025.
Notably, the patent application was submitted under the International Patent Classification (IPC) system, which is managed by the World Intellectual Property Organization (WIPO).
Inventor(s): CARRIE, Romain (Safranc/o Centre d'Excellence Propriete IntellectuelleRond-point ene Ravaud, Reau77550 MOISSY-CRAMAYEL)
Abstract:
The invention relates to a method (101) for detecting fr...