GENEVA, Dec. 22 -- MTU AERO ENGINES AG (Dachauer StraBe 66580995 Munchen) filed a patent application (PCT/EP2025/065682) for "SUPERALLOY FILLER, BRAZING MIXTURE, AND METHOD FOR BRAZING A COMPONENT" on Jun 05, 2025. With publication no. WO/2025/257025, the details related to the patent application was published on Dec 18, 2025.
Notably, the patent application was submitted under the International Patent Classification (IPC) system, which is managed by the World Intellectual Property Organization (WIPO).
Inventor(s): REKER, Dirk Wilhelm (c/o MTU Aero Engines AGDachauer Strasse 66580995 Munchen), SOWA, Roman (c/o MTU Aero Engines AGDachauer Strasse 66580995 Munchen), SCHWALBE, Caspar (c/o MTU Aero Engines AGDachauer Strasse 66580995 Munchen)...