GENEVA, Dec. 10 -- LG ENERGY SOLUTION, LTD. (Tower1, 108, Yeoui-daero,Yeongdeungpo-gu,Seoul 07335), 주식회사 엘지에너지솔루션 (서울특별시영등포구여의대로 108, 타워1) filed a patent application (PCT/KR2025/003322) for "ELECTRODE SURFACE ANALYSIS METHOD AND ELECTRODE SURFACE ANALYSIS SYSTEM" on Mar 14, 2025. With publication no. WO/2025/249722, the details related to the patent application was published on Dec 04, 2025.

Notably, the patent application was submitted under the International Patent Classification (IPC) system, which is managed by the World Intellectual Property Organiz...