GENEVA, Oct. 6 -- CORNING INCORPORATED (One Riverfront PlazaCorning, New York 14831) filed a patent application (PCT/US2025/017465) for "METAL FLUORIDE AND PLASMA ASSISTED ATOMIC LAYER DEPOSITION COATING" on Feb 27, 2025. With publication no. WO/2025/207260, the details related to the patent application was published on Oct 02, 2025.
Notably, the patent application was submitted under the International Patent Classification (IPC) system, which is managed by the World Intellectual Property Organization (WIPO).