GENEVA, Feb. 25 -- INDUSTRY-UNIVERSITY COOPERATION FOUNDATION HANYANG UNIVERSITY ERICA CAMPUS (55 Hanyangdaehak-roSangnok-gu, Ansan-siGyeonggi-do 15588), 한양대학교 에리카산학협력단 (경기도안산시 상록구한양대학로 55) filed a patent application (PCT/KR2024/095929) for "AREA SELECTIVE ATOMIC LAYER DEPOSITION METHOD, APPARATUS THEREFOR, AND HZO MATERIAL FILM STRUCTURE MANUFACTURED THEREBY" on Jul 23, 2024. With publication no. WO/2025/037954, the details related to the patent application was published on Feb 20, 2025.
Notably, the patent application was submitted under the Internatio...