GENEVA, Nov. 23 -- HUAZHONG UNIVERSITY OF SCIENCE AND TECHNOLOGY (No.1037 Luoyu Road, Hongshan DistrictWuhan, Hubei 430074), 华中科技大学 (中国湖北省武汉市洪山区珞喻路1037号) filed a patent application (PCT/CN2025/072509) for "PREPARATION APPARATUS AND METHOD FOR CALIBRATED TEST BLOCK WITH STRESS CORROSION CRACKS FOR NON-DESTRUCTIVE TESTING" on Jan 15, 2025. With publication no. WO/2025/236740, the details related to the patent application was published on Nov 20, 2025.

Notably, the patent application was submitted under the International Patent Classification (IPC) system, which is managed by the World Intellectual...