GENEVA, June 1 -- CONTEMPORARY AMPEREX TECHNOLOGY CO., LIMITED (No. 2 Xingang Road, Zhangwan, Jiaocheng District,Ningde, Fujian 352100), 宁德时代新能源科技股份有限公司 (中国福建省宁德市蕉城区漳湾镇新港路2号) filed a patent application (PCT/CN2024/079760) for "WELDING DEFECT DETECTION METHOD AND APPARATUS, AND STORAGE MEDIUM AND PROGRAM PRODUCT" on Mar 01, 2024. With publication no. WO/2025/107442, the details related to the patent application was published on May 30, 2025.